Figure 5

(A) Time dependent changes in optical density at 400 nm of ABMDMA irradiated (control 1), ABMDMA-QD without irradiation (control 2), ABMDMA-AIS irradiated and ABMDMA-AIS@ZnS irradiated after the time periods (0, 20, 40, 60, 80, 100, 120, 140 and 160 min). (B) Shows the exponential decay fitted curve with respect to time.