Figure 2 | Scientific Reports

Figure 2

From: Moderate fabrication and characterization of the microcrystalline Sr2CuO3 glass films with effective nonlinearities

Figure 2

(a) Comparison of powder XRD patterns of the microcrystalline Sr2CuO3 glass films with different sintering temperatures (1) 100 °C, (2) 200 °C, (3) 300 °C, (4) 400 °C, (5) 500 °C and (6) 600 °C. (b) Comparison of powder XRD patterns of the microcrystalline Sr2CuO3 glass films polished different times under 500 °C sintering (1) 0 min, (2) 60 min, (3) 100 min, (4) 140 min and (5) 180 min.