Table 3 Effects of active materials loading and current density on areal capacity (delithiation) performance for C-SCVH+W conducted between 0.002 V to 1.5 V.

From: Mechanochemical synthesis of Si/Cu3Si-based composite as negative electrode materials for lithium ion battery

Loading (mg cm−2)

Current density (mAh g−1)

1st areal capacity (mAh cm−2)

100th areal capacity (mAh cm−2)

Retention (%)

0.8

200

1.28

1.14

89.1

2.3

100

4.08

3.31

81.1

2.3

200

3.68

2.69

73.1