Figure 2 | Scientific Reports

Figure 2

From: High conductivity of ultrathin nanoribbons of SrRuO3 on SrTiO3 probed by infrared spectroscopy

Figure 2

Reflectance measured at 300 K on the SRO/STO unpatterned sample A, having a SRO thickness d = 6 nm, in the same two polarizations that were then used on the striped samples B, C and D (red and blue curves). The open circles show the fit to reflectivity data described in the text, which provides the real part σ1 of the optical conductivity displayed in the inset.