Figure 3
From: Effects of Precipitates Evolution on Low Stress Creep Properties in P92 Heat-resistant Steel

SEM-EDS diagrams of bright particles A (a) and dark particles B (b) in P92 heat-resistant steels following thermal aging for 3000 h.
From: Effects of Precipitates Evolution on Low Stress Creep Properties in P92 Heat-resistant Steel

SEM-EDS diagrams of bright particles A (a) and dark particles B (b) in P92 heat-resistant steels following thermal aging for 3000 h.