Table 1 Saturation magnetization and coercivity values for the AlCoFeNi and AlCo0.5Cr0.5FeNi alloys for the different heat-treated conditions.

From: Influence of Cr Substitution and Temperature on Hierarchical Phase Decomposition in the AlCoFeNi High Entropy Alloy

Alloy

Heat treatment

Ms (emu/g)

Hc (Oe)

AlCoFeNi

600 °C/15 h

99.8

14.5

AlCoFeNi

1000 °C/15 h

111.6

4.3

AlCo0.5Cr0.5FeNi

600 °C/15 h

46.2

95.6

AlCo0.5Cr0.5FeNi

1000 °C/15 h

42.2

39.4