Figure 3
From: An unconventional hydrogen effect that suppresses thermal formation of the hcp phase in fcc steels

(a) Cooling and aging pattern and (b) XRD profiles at each cycle with hydrogen pre-charging at 353 K. The aging times given in (b) indicate total aging time.