Figure 10

(a–c) Inverse pole figure maps and (d–f) corresponding inverse pole figures of the extruded alloy (processed at 350 °C and 1 mm/s) after annealing at various temperatures for 10 min: (a,d) 350 °C, (b,e) 400 °C and (c,f) 450 °C.

(a–c) Inverse pole figure maps and (d–f) corresponding inverse pole figures of the extruded alloy (processed at 350 °C and 1 mm/s) after annealing at various temperatures for 10 min: (a,d) 350 °C, (b,e) 400 °C and (c,f) 450 °C.