Table 1 Fitted EIS results of A283-D steel in highly compacted bentonite with 30% water content at different temperatures.

From: Long term corrosion estimation of carbon steel, titanium and its alloy in backfill material of compacted bentonite for nuclear waste repository

Temperature(°C)

Rs(Ω·cm2)

Rb(Ω·cm2)

Rct(Ω·cm2)

90

46.52

15.18

2.14 × 103

80

57.51

16.61

5.88 × 103

70

51.71

21.02

1.47 × 104

55

48.40

37.40

3.80 × 104

40

71.28

40.53

2.82 × 104

25

139.90

51.02

2.71 × 104