Figure 7

Comparative gravimetric capacitance and areal capacitance of rGO/MnFe2O4, rGO/MnFe2O4/Ppy, rGO/NiFe2O4 and rGO/NiFe2O4/Ppy nanocomposites at 5 mVs−1.

Comparative gravimetric capacitance and areal capacitance of rGO/MnFe2O4, rGO/MnFe2O4/Ppy, rGO/NiFe2O4 and rGO/NiFe2O4/Ppy nanocomposites at 5 mVs−1.