Figure 5
From: Strong and ductile AZ31 Mg alloy with a layered bimodal structure

EBSD maps of (a) 180 °C and (b) 400 °C -ARB samples after tensile test and (c) 180 °C and (d) 400 °C -HR samples after tensile test.