Figure 4

TEM pictures, EDX, and particle size distribution of ZrO2 and Al2O3 for the compositions with following Al amount: 10 mol.% (a–c), 50 mol.% (d–f), 70 mol.% (g–i), 90 mol.% (j–l) of Al, after annealing at 1500 oC.

TEM pictures, EDX, and particle size distribution of ZrO2 and Al2O3 for the compositions with following Al amount: 10 mol.% (a–c), 50 mol.% (d–f), 70 mol.% (g–i), 90 mol.% (j–l) of Al, after annealing at 1500 oC.