Table 1 PEEK annealing procedure.
From: A miniaturized spectrometer for NMR relaxometry under extreme conditions
Start temp (°C) | End temp (°C) | Ramp rate (°C/min) | Duration (hrs) |
|---|---|---|---|
20 | 150 | 0.1 | 21.7 |
150 | 150 | 0 | 3 |
150 | 200 | 0.1 | 8.3 |
200 | 200 | 0 | 3 |
200 | 20 | −0.1 | 30 |
From: A miniaturized spectrometer for NMR relaxometry under extreme conditions
Start temp (°C) | End temp (°C) | Ramp rate (°C/min) | Duration (hrs) |
|---|---|---|---|
20 | 150 | 0.1 | 21.7 |
150 | 150 | 0 | 3 |
150 | 200 | 0.1 | 8.3 |
200 | 200 | 0 | 3 |
200 | 20 | −0.1 | 30 |