Table 2 The paramerters of Drude model.

From: Phase-change like process through bond switching in distorted and resonantly bonded crystal

 

σDC(Ω−1cm−1)

ωp (eV)

γ (eV)

Non-bent

3110

2.298

0.229

Weakly bent

2920

2.151

0.213

bent

2650

2.001

0.203

Strong bent

2320

1.697

0.167