Table 3 Chemical compositions of investigated alloys [wt.%].
From: Quantitative approach to realization of ultrasonic grain refinement of Al-7Si-2Cu-1Mg alloy
Pouring temperature (°C) | UST | Si | Fe | Cu | Mn | Mg | Ti | Zr | Al |
|---|---|---|---|---|---|---|---|---|---|
620 | X | 6.9 | 0.14 | 2.1 | 0.006 | 1.12 | 0.02 | 0.01 | Bal. |
O | 6.8 | 0.15 | 2.1 | 0.005 | 1.08 | 0.02 | 0.01 | Bal. | |
650 | X | 6.8 | 0.14 | 2.2 | 0.006 | 1.11 | 0.02 | 0.01 | Bal. |
O | 6.7 | 0.14 | 2.2 | 0.004 | 1.08 | 0.02 | 0.01 | Bal. | |
700 | X | 6.8 | 0.13 | 2.1 | 0.005 | 1.09 | 0.02 | 0.01 | Bal. |
O | 6.9 | 0.15 | 2.1 | 0.005 | 1.07 | 0.02 | 0.01 | Bal. | |
785 | X | 7.1 | 0.16 | 2.1 | 0.005 | 1.05 | 0.02 | 0.01 | Bal. |
O | 6.8 | 0.16 | 2.0 | 0.005 | 1.06 | 0.02 | 0.01 | Bal. |