Figure 3

Hk variation with free layer thickness and temperature. (a) Hk dependence on nominal CFB thickness measured using FMR at 35 °C and 85 °C, with and without an Mg insertion layer. (b) Hk dependence on nominal Mg thickness measured using FMR at 35 °C and 85 °C.