Figure 2 | Scientific Reports

Figure 2

From: Crystallization Mechanism in Spark Plasma Sintered Bulk Metallic Glass Analyzed using Small Angle Neutron Scattering

Figure 2

(a,b) Transmission electron microscope dark field images and (c,d) corresponding selected area diffraction patterns of spark plasma sintered iron based metallic glass annealed at 700 °C and 725 °C for 100 min. Regions of brighter contrast in (a,b) represent crystals embedded within the metallic glass matrix that exhibit a range of diameter from 10 to 30 nm.

Back to article page