Table 2 Compression and bending properties of control bone cements after one day storage in room temperature, 23 ± 1 °C (Dry sample) and distilled water, 37 ± 1 °C (Wet sample) (Mean (SD), n = 5).
Properties | Compressive strength (MPa) | Compressive modulus (GPa) | Flexural strength (MPa) | Flexural modulus (GPa) |
|---|---|---|---|---|
Dry sample | 89.88 (0.9) | 1.72 (0.05) | 57.33 (3.24) | 2.65 (0.04) |
Wet sample | 83.21 (1.04) | 1.61 (0.06) | 49.79 (4.47) | 2.35 (0.04) |