From: Solid-electrolyte interphase nucleation and growth on carbonaceous negative electrodes for Li-ion batteries visualized with in situ atomic force microscopy

Figure 6

CV curve and corresponding AFM topography images recorded on LiCo1/3Ni1/3Mn1/3O2 in 1 M LiPF6 in EC/DMC = 50/50 (v/v) electrolyte solution at 2 mV/s cycling rate vs Li+/Li. LiCo1/3Ni1/3Mn1/3O2 before (a) and after (b) cycling. 4 × 4 µm squares in (a) and (b) depict in situ scan areas shown in (c).