Table 1 Reported main parameters for 3D printed OECT in literatures: channel dimensions, gmax, ION/IOFF. ND indicates not declared parameter.
From: Rapid prototyping of 3D Organic Electrochemical Transistors by composite photocurable resin
Fabrication Techniques | Channel dimension W/L/t (μm) | Materials | gmax (mS) | ION/IOFF | References |
|---|---|---|---|---|---|
Stereolithopgraphy | 700/1900/500 | PEGDA:PEDOT | 2.5 | 2.79 ± 1.6 ⋅103 | This work |
Aerosol-jet printing | 200/200/0.2 | PEDOT:PSS | 0.52 | ND | Ref.19 |
Laser sintering | 1,000/15,000/1,000 | PEDOT:PSS | 2 | 2 | Ref.20 |
FDM/direct writing 3D | 1,000/1,600/7.1 | PEDOT:PSS | 31.8 | 1.33â‹…103 | Ref.21 |
Syringe deposition | 3,000/3,000/5 | PEDOT:PSS | ND | 2 | Ref.23 |
Melt extrusion/electrospining | 200/1,500/200 | PEDOT:Nafion | 30–40 | 100 | Ref.38 |