Figure 8

Cell viability (absorbance at 450 nm) of hFOB 1.19 cells exposed to SeB-NPs and AgSB-NPs using different concentrations, which was measured by the CCK-8 assay, (a): SeB1; (b): SeB2; (c): SeB3; (d): AgSeB1; (e): AgSeB2; (f): AgSeB3. Without adding nanoparticles as a control group (CK).