Figure 3

(a–g) Angular dependence of the THG intensity on the incident linear polarization for seven GeAs flakes with the thicknesses of 11 nm, 28 nm, 49 nm, 71 nm, 119 nm, 129 nm and 155 nm. Black squares, red circles and blue triangles refer to the measured x-component, y-component and total intensity of THG signal, respectively. Solid curves represent the corresponding theoretical fittings. (h) Evolution of the measured anisotropy ratio and THG conversion efficiency as a function of the flake thickness under the pump irradiance of 8.4 GW/cm2.