Figure 10

Surface morphologies (a) and cross-sectional morphologies (b) of the pre-oxidized samples under a solid NaCl deposit layer in humid O2 for 5 h at 600 ˚C.

Surface morphologies (a) and cross-sectional morphologies (b) of the pre-oxidized samples under a solid NaCl deposit layer in humid O2 for 5 h at 600 ˚C.