Table 9 Vertical distance of experimental data points from the selective cross-link scission curve.

From: Devulcanization of ground tire rubber: microwave and thermomechanical approaches

Sample

The vertical distance from the selective scission curve (%)

dGTR_MW_50g

53.8

dGTR_MW_50g_1

59.7

dGTR_MW_50g_2

75.0

dGTR_MW_100g

51.9

dGTR_MW_100g_1

67.2

dGTR_MW_100g_2

88.3

GTR_H_2

77.0

dGTR_TM_40/160

13.5

dGTR_TM_40/170

26.8

dGTR_TM_40/180

28.5

dGTR_TM_40/190

30.6

dGTR_TM_40/200

35.4

dGTR_TM_120/160

20.0

dGTR_TM_120/170

44.3

dGTR_TM_120/180

45.5

dGTR_TM_120/190

31.5

dGTR_TM_120/200

45.4