Table 1 Summary of related photocatalyst systems for phenol degradation.
Photocatalyst | Light source | Phenol (ppm) | K (h−1) | Degradation (%) | Mineralization (%) | References |
|---|---|---|---|---|---|---|
Bi2WO6/BiOCl 1 g/L | 500 W Xe | 20 | 0.59 | 93% (5 h) | 79.4% | This work |
C60/BiOCl 1 g/L | 500 W Xe | 20 | 0.26 | 97% (12 h) | – | |
BiOCl/Bi12O17Cl2 0.6 g/L | 500 W Xe | 10 | – | 46% (4 h) | – | |
PDI/Bi2WO6 0.5 g/L | 500 W Xe > 420 nm | 5 | 0.36 | 67% (2 h) | – | |
BiOBr0.9I0.1/BiOI 0.8 g/L | 500 W Xe > 420 nm | 10 | 0.088 | 50% (8 h) | ||
TiO2/BiOCl 1 g/L | 300 W Xe > 450 nm | 50 | – | 55% (6 h) | 50% | |
BiOCl/Bi2MoO6 1 g/L | 300 W Xe > 420 nm | 10 | – | 40% (4 h) | – | |
Bi2WO6/RGO 0.5 g/L | Natural sunlight | 10 | – | 65% (8 h) | 39.7% |