Figure 9

Variation of storage modulus of MRE samples towards frequency sweeps, containing spherical (filled symbol) and plate-like (unfilled symbol) CIPs, at different corrosion conditions of (a) 0, (b) 0.5, (c) 1.0 and (d) 1.5 vol.% HCl, under different applied magnetic fields.