Figure 7
From: Roles of the semisolid heating on the microstructure of a hypereutectic Al–Fe–Cu alloy

the quenched microstructure and EDS of Al–Fe–Cu alloy reheated at 630 °C for 40 min, deep etched. (a) Microstructure; (b) α-Al grain; (c) Fe-rich phase; (d) Cu-rich zone.