Table 1 Crystallite sizes obtained using the Scherrer formula and the texture coefficients for the deposited CeO2 films.

From: Strong texture tuning along different crystalline directions in glass-supported CeO2 thin films by ultrasonic spray pyrolysis

Sample

Crystallite size (nm)

Texture coefficient

(111)

(200)

(220)

(311)

(111)

(200)

(220)

(311)

0.03-HF-475

17

41

20

21

0.4

2.2

0.5

0.9

0.03-HF-425

15

24

25

2.1

0.1

0.3

0.6

0.02-HF-475

20

72

40

44

0.2

3.1

0.2

0.5

0.03-LF-475

16

19

19

18

1.1

1.0

1.1

0.9