Table 2 Experimental process parameters.
Process parameters | Value |
|---|---|
Laser power P | 200 W |
Scanning speed v | 1000 mm/s |
Scanning distance m | 0.06 mm |
Thickness of powder layer H | 0.035 mm |
Process parameters | Value |
|---|---|
Laser power P | 200 W |
Scanning speed v | 1000 mm/s |
Scanning distance m | 0.06 mm |
Thickness of powder layer H | 0.035 mm |