Figure 7

POM images of CLC layer with the defect lines formed nearly parallel to the rubbing direction R under \(V = 1.3\) V (a) and in 9.2 s (b), 46.8 s (c) after switching off the field. The analyzer is oriented to the polarizer at 40\(^\circ\) angle.