Figure 10

ATR FTIR spectra of PMMA polymer before and after plasma treatment measured in a wavenumber interval of 4000–400 cm−1. Argon flow rate 20 NL/min. Microwave power 460 W.

ATR FTIR spectra of PMMA polymer before and after plasma treatment measured in a wavenumber interval of 4000–400 cm−1. Argon flow rate 20 NL/min. Microwave power 460 W.