Table 2 Porous properties of the beads using nitrogen adsorption before and after polymer modification.
Pore diameter (nm) | Beads | Surface area (m2/g) | Total pore volume (cm3/g) | Peak pore diameter (nm) |
|---|---|---|---|---|
7 | Aminopropyl silica beads | 169 | 0.331 | 10.8 |
P(NIPAAm-co-BMA)-modified beads | 159 | 0.460 | 8.31 | |
12 | Aminopropyl silica beads | 252 | 0.910 | 14.1 |
P(NIPAAm-co-BMA)-modified beads | 180 | 0.568 | 12.6 | |
30 | Aminopropyl silica beads | 99.0 | 0.680 | 27.3 |
P(NIPAAm-co-BMA)-modified beads | 94.3 | 0.568 | 24.1 |