Table 1 Percent yield and proximate analysis of eucalyptus wood chips and activated carbon.
Sample | Moisture (wt%) | Volatile matter (wt%) | Ash (wt%) | Fixed carbon (wt%) | %yield |
|---|---|---|---|---|---|
Raw eucalyptus wood chips | 7.89 ± 0.22 | 20.87 ± 0.22 | 1.93 ± 1.18 | 68.93 ± 0.09 | – |
Activated carbon at 500 °C | 2.63 | 5.95 | 1.59 | 70.32 | 31.79 ± 0.70 |
Activated carbon at 600 °C | 1.54 | 3.2 | 1.43 | 79.23 | 25.84 ± 0.37 |
Activated carbon at 700 °C | 1.16 | 0.89 | 1.04 | 80.54 | 21.63 ± 1.52 |