Table 1 DSC results for struvite → dittmarite conversion process.
From: First experimental evidence of the piezoelectric nature of struvite
Heating rate [K/min] | Ts [K] | Tmax [K] | Tt [K] | H [J/g] |
|---|---|---|---|---|
0.4 | 366.5 | 381.0 | 386.9 | − 287.8 |
1.2 | 374.0 | 388.9 | 393.1 | − 295.5 |
2.0 | 378.5 | 391.0 | 398.8 | − 312.2 |