Table 5 Ti6Al4V and tool parameters used in the FEM simulations.
From: Modeling of the fracture energy on the finite element simulation in Ti6Al4V alloy machining
Mechanical and thermal properties for Ti6Al4V | |
Density (t/mm3) | 4.5E−09 |
Young’s modulus (MPa) | 144,000 |
Poisson’s ratio | 0.32 |
Expansion coefficient (m/m K) | 9.40E−06 |
Specific heat (J/kg) | 656 |
Thermal conductivity (W/m K) | 6.6 |
Melting point (K) | 1933 |
Thermal and mechanical properties of the cutting tool | |
Density (t/mm3) | 1.19E−08 |
Young’s modulus (MPa) | – |
Poisson’s ratio | |
Expansion coefficient (m/m K) | |
Specific heat (J/kg) | 33,700,000 |
Thermal conductivity (W/m K) | 86 |