Figure 20
From: ZrN-ZrOxNy vs ZrO2-ZrOxNy coatings deposited via unbalanced DC magnetron sputtering

Optical micrograph of the proliferation of osteoblast primary (a) uncoated AISI 316L and (b) ZrO2-ZrOxNy-316L system at 72 h. Images of fluorescence microscopy (c) uncoated AISI 316L and (d) ZrO2-ZrOxNy-316L system at 72 h with a filter; (e) and (f) culture cells derived from the mouse cranial vault C57BL/6 at 24 h on ZrO2-ZrOxNy-316L system.