Table 1 Tests results of UHPFRCs cured at room temperature.
References | Dimensions | Test types | Results MPa |
|---|---|---|---|
Prismatic specimens (40 × 40 × 160 mm3) | Flexural strength | 23 | |
Cylindrical specimens (100 × 200 mm3) | Compressive strength | 163 | |
Prismatic specimens (40 × 40 × 160 mm3) | Flexural strength | 27.8 | |
Cubic specimens (50 × 50 × 50 mm3) | Compressive strength | 110 | |
Cubic specimens (50 × 50 × 50 mm3) | Compressive strength | 125 | |
Prismatic specimens (50 × 50 × 200 mm3) | Flexural strength | 22 | |
Cylindrical specimens (R = 50 mm H = 100 mm) | Compressive strength | 162 | |
Plate specimens (100 × 12 × 400 mm3) | Flexural strength | 35 | |
Beam specimens (100 × 100 × 400 mm3) | Tensile strength | 23 | |
Prismatic specimens (50 × 200 × 500 mm3) | Compressive strength | 168 | |
Tensile strength | 11 |