From: Optimization studies of stir casting parameters and mechanical properties of TiO2 reinforced Al 7075 composite using response surface methodology

Figure 8

Microstructural images of developed composite showing different conditions of experimental runs at temperature, speed, and time values of (a) 700 °C, 500 rpm, 15 min; (b) 350 °C, 331.821 rpm, 10 min; (c) 868.179 °C, 500 rpm, 15 min; (d) 800 °C, 600 rpm, 20 min; (e) 800 °C, 600 rpm, 10 min; (f) 800 °C, 600 rpm, 20 min.