Table 1 Summary of the nonlinear properties of each of the SA devices.
SA Device | Modulation depth (%) | Saturation intensity (MW/cm2) |
|---|---|---|
Ta2AlC-deposited tapered fiber | 6.02 | 0.36 |
Ta2AlC-deposited SPF | 1.09 | 1.63 |
Ta2AlC-deposited arc-shaped fiber | 0.82 | 1.03 |