Table 2 The % Area and FWHM of overlapping peaks present in deconvoluted HF Raman band of respective surface scratch grooves.
From: Revealing the surface structural cause of scratch formation on soda-lime-silica glass
Peak label | Normalized integrated area (%) | FWHM (cm−1) | ||
|---|---|---|---|---|
Untreated | Heat-treated | Untreated | Heat-treated | |
Q1 | 16.7 | 1 | 82 | 24 |
Q2 | 10.4 | 13 | 56 | 182 |
ν Si–O | 2.6 | 52.5 | 31 | 200 |
Q3 | 56.2 | 31 | 83 | 84 |
Q4 | 14.1 | 2.5 | 90 | 44 |