Table 4 The specific surface area before and after the treatment of AMD with biologically activated lignite immobilized SRB particles.
Langmuir specific surface area (m2/g) | BET specific surface area (m2/g) | BET molecular cross-sectional area (nm2) | BET correlation coefficient | Langmuir correlation coefficient | |
|---|---|---|---|---|---|
Before the reaction | 16.6545 | 7.4621 | 0.1620 | 0.9990 | 0.9860 |
After the reaction | 25.5604 | 11.8146 | 0.1620 | 0.9990 | 0.9860 |