Table 2 The performance parameters of different graphene content.

From: Mechanical performance of graphenex/poly(ether ketone ketone) composite sheets by hot pressing

No

Context

Maximum conductivity(S/n)

Tm (°C)

Tg (°C)

Sinter temperature (°C)

1

PEKK

0

317

145

177

2

2%Graphene

0

289

144

177

3

3%Graphene

0.001

300

148

210

4

4%Graphene

0.009

323

205

210

5

5%Graphene

0.164

295

134

210

6

6%Graphene

0.126

302

210

240