Figure 6

Results of temperature profiles at the center of the slab from experimental and modelling approaches: (a) 10 mm sample vulcanized at 150 °C; (b) 10 mm sample vulcanized at 180 °C; (c) 30 mm sample vulcanized at 150 °C; (d) 30 mm sample vulcanized at 180 °C.