Table 4 Simulation results of the maximum rate of reaction at the center of each slab.

From: A new modelling approach for predicting process evolution of cork-rubber composites slabs vulcanization

Vulcanization temperature (°C)

Thickness (mm)

Maximum rate of reaction (s−1)

150

10

2.95 × 10–3

150

30

2.84 × 10–3

180

10

21.85 × 10–3

180

30

8.17 × 10–3