From: RETRACTED ARTICLE: Strontium doped bioglass incorporated hydrogel-based scaffold for amplified bone tissue regeneration

Figure 5

SEM images of scaffolds surface for evaluating biomineralization. (a) Alg/Cs, (b) Alg/Cs/BG30 and (c) Alg/Cs/Sr-BG30 scaffolds, (I) before submerging, (II) after 7 days submerging (100 μm scale), (III) after 7 days submerging (30 μm scale), (IV) after 14 days submerging (100 μm scale), (V) after 14 days submerging (30 μm scale).