Figure 3

XRD patterns of the Mg–15Gd–1Zn alloy under different sintering conditions: (a) at 430 °C; (b) at 450 °C; (c) at 470 °C; (d) the RS ribbon and its as-cast ingot.

XRD patterns of the Mg–15Gd–1Zn alloy under different sintering conditions: (a) at 430 °C; (b) at 450 °C; (c) at 470 °C; (d) the RS ribbon and its as-cast ingot.