Table 2 Fit results of EXAFS data of H2O2-Pt/Ti–FS at the Pt L3 edge.

From: Dispersion and stability mechanism of Pt nanoparticles on transition-metal oxides

T ( °C)

Pt–O

Pt-Pt(1)

Pt-Pt(2)

N

d (Å)

σ22)

N

d (Å)

σ22)

N

d (Å)

σ22)

RT

5.7(7)

2.003(7)

0.003(1)

   

8(1)

3.28(1)

0.018(2)

100

5.7(7)

2.010(7)

0.004(1)

   

8(1)

3.22(4)

0.026(5)

150

3.8(7)

2.016(7)

0.004(1)

2(1)

2.75(1)

0.014(1)

6(1)

3.05(1)

0.024(2)

200

1(1)

2.05(1)

0.006(1)

8(1)

2.719(7)

0.014(1)

   

250

   

7.9(8)

2.713(6)

0.012(1)

   

300

   

7.6(8)

2.702(7)

0.012(1)

   

350

   

7.2(8)

2.699(7)

0.011(1)

   

400

   

6.8(8)

2.702(8)

0.011(1)

   

450

   

7.2(8)

2.708(8)

0.013(1)

   

500

   

7.8(9)

2.702(7)

0.014(1)

   

RTc

   

7.6(9)

2.730(8)

0.008(1)

   
  1. Data are shown in Fig. 4b.