Figure 5

Results of EDS analysis performed on samples with Ni–Mo alloy coatings deposited from DES + 0.2 mol dm−3 NiCl2 + 0.01 mol dm−3 (NH4)6Mo7O24 at − 0.5, − 0.6, − 0.7, − 0.8, − 0.9 V vs. Ag for 60 min at 50 °C.

Results of EDS analysis performed on samples with Ni–Mo alloy coatings deposited from DES + 0.2 mol dm−3 NiCl2 + 0.01 mol dm−3 (NH4)6Mo7O24 at − 0.5, − 0.6, − 0.7, − 0.8, − 0.9 V vs. Ag for 60 min at 50 °C.