Table 1 Corrosion parameters (Ecorr, icorr, βc, βa) determined from the potentiodynamic curves of the Ni–Mo alloy coatings recorded after 24 h of exposure of the samples in 0.05 mol dm−3 NaCl solution.

From: Electrodeposition of Ni–Mo alloy coatings from choline chloride and propylene glycol deep eutectic solvent plating bath

Deposition potential (E, V vs Ag)

Ecorr [V vs. Ag|AgCl]

icorr [μA cm−2]

βc [mV dec−1]

βa [mV dec−1]

− 0.5 V

− 0.136

0.21

78

108

− 0.6 V

− 0.284

0.23

71

80

− 0.7 V

− 0.219

0.29

129

86

− 0.8 V

− 0.219

0.13

76

63

− 0.9 V

− 0.201

0.24

93

71