Table 1 ZnO crystallite size before and after irradiated with lasers having wavelengths of \(532 nm\) and \(1064 nm\).
Samples | hkl (1 0 1) | Grain size DTEM (nm) | ||||
|---|---|---|---|---|---|---|
2θ (°) | β (deg.) | DXRD (nm) | \(\delta (\times {10}^{-4} {nm}^{-2})\) | \(\varepsilon (\times {10}^{-4} )\) | ||
pure | 36.5358 | 0.62340 | 13.4198 | 55.5274 | 25.8300 | 46 |
Irradiated by 1064 nm | 36.3945 | 0.58190 | 14.3710 | 48.4201 | 24.1203 | 45 |